Lanthanum aluminate by atomic layer deposition and molecular beam epitaxy

  • D. H. Triyoso
  • , H. Li
  • , R. I. Hegde
  • , Z. Yu
  • , K. Moore
  • , J. Grant
  • , B. E. White
  • , P. J. Tobin

Research output: Contribution to journalArticlepeer-review

12 Scopus citations

Abstract

A comparison of physical and electrical characteristics of lanthanum aluminate (LAO) dielectrics formed by atomic layer deposition (ALD) and molecular beam epitaxy (MBE) is investigated in this study. Physical characteristics of LAO deposited with these two deposition methods are compared using x-ray photoelectron spectroscopy (XPS), transmission electron microscopy (TEM), and secondary ion mass spectrometry (SIMS). Capacitors with TaN and TaSiN gate electrodes were fabricated to assess electrical properties of these LAO films. ALD LAO was deposited using La [N (SiMe3) 2] 3, Al (CH3) 3 and water at 225-275 °C. ALD LAO is stable against Pt and TiNW metal gates up to 800 °C. After annealing at 900 °C, interactions between metal gates and dielectrics are observed resulting in nonfunctional devices. MBE LAO film was deposited at room temperature or 200-400 °C in two ways: Using single element targets (La, Al) or a compound target. The LAOTaN stack deposited with single element targets showed significant Si up diffusion from the substrate to the dielectric and the metal gate electrode. In addition, nitrogen diffusion from the metal gate into the dielectric was detected. The LAOTaN stack deposited with a compound target showed improved thermal stability. No metal out-diffusion and only very slight Si out diffusion was detected after a 900 °C anneal. LAO capacitors show well-behaved capacitance-voltage and leakage current density-voltage characteristics. These results indicate that the method by which lanthanum aluminate films are deposited strongly influenced their thermal stability. Of all the films examined, the most stable films are deposited by MBE using a compound target.

Original languageEnglish
Pages (from-to)2480-2485
Number of pages6
JournalJournal of Vacuum Science and Technology B: Microelectronics and Nanometer Structures
Volume23
Issue number6
DOIs
StatePublished - Nov 2005

Fingerprint

Dive into the research topics of 'Lanthanum aluminate by atomic layer deposition and molecular beam epitaxy'. Together they form a unique fingerprint.

Cite this