Vortex phase diagram and Jc limiting factor in high Tc Bi2Sr2Ca2Cu3O10/Ag superconducting tapes

  • Qiang Li
  • , H. J. Wiesmann
  • , M. Suenaga
  • , L. Motowidlo
  • , P. Haldar
  • Brookhaven National Laboratory
  • Inc.
  • Intermagnetics General Corporation

Research output: Contribution to journalArticlepeer-review

18 Scopus citations

Abstract

Based on our detailed measurements of current-voltage characteristics for a Bi2Sr2Ca2Cu3O10/Ag tape (Jc≅2×104 A/cm2 at 77 K and zero field) immersed in liquid neon (27 K) and in liquid oxygen (54-90 K) as a function of applied magnetic field up to 17 T, we extended the vortex phase diagram of superconducting Bi2Sr2Ca2Cu3O10 in the mixed state and show that Jc for this tape at T≥27 K in magnetic field (except at very low field) is fundamentally limited by the transition of the vortex-solid-to-liquid within grains rather than the dissipation from grain boundaries.

Original languageEnglish
Pages (from-to)637
Number of pages1
JournalApplied Physics Letters
Volume66
Issue number5
DOIs
StatePublished - 1995

Fingerprint

Dive into the research topics of 'Vortex phase diagram and Jc limiting factor in high Tc Bi2Sr2Ca2Cu3O10/Ag superconducting tapes'. Together they form a unique fingerprint.